« Previous
Next »
Dental Materials
Volume 26, Issue 4
, Pages 380-386
, April 2010
One-year stability of resin–dentin bonds created with a hydrophobic ethanol-wet bonding technique
References
- . Early and 24-hour bond strength and degree of conversion of etch-and-rinse and self-etch adhesives. Am J Dent. 2008;21:30–34
- Microtensile bond strength of eleven contemporary adhesives to dentin. J Adhes Dent. 2001;3:237–245
- . In vitro degradation of resin–dentin bonds analyzed by microtensile bond test, scanning and transmission electron microscopy. Biomaterials. 2003;24:3795–3803
- . Degradation patterns of different adhesives and bonding procedures. J Biomed Mater Res B Appl Biomater. 2003;66:324–330
- . Durability of resin–dentin bonds related to water and oil storage. Am J Dent. 2005;18:315–319
- Four-year water degradation of total-etch adhesives bonded to dentin. J Dent Res. 2003;82:136–140
- . One-year clinical performance of a self-etching adhesive in class V resin composites cured by two methods. Oper Dent. 2002;27:218–222
- . Clinical effectiveness of contemporary adhesives: a systematic review of current clinical trials. Dent Mater. 2005;21:864–881
- Single-bottle adhesives behave as permeable membranes after polymerization. I. In vivo evidence. J Dent. 2004;32:611–621
- . Have dentin adhesives become too hydrophilic?. J Can Dent Assoc. 2003;69:726–731
- From dry bonding to water-wet bonding to ethanol-wet bonding. A review of the interactions between dentin matrix and solvated resins using a macromodel of the hybrid layer. Am J Dent. 2007;20:7–20
- . Water absorption of poly(methyl methacrylate) containing 4-methacryloxyethyl trimellitic anhydride. Biomaterials. 2003;24:1381–1387
- Effect of resin hydrophilicity and temperature on water sorption of dental adhesive resins. Biomaterials. 2006;27:1695–1703
- Effect of resin hydrophilicity and water storage on resin strength. Biomaterials. 2004;25:5789–5796
- Effects of resin hydrophilicity on water sorption and changes in modulus of elasticity. Biomaterials. 2005;26:6449–6459
- Effect of simulated pulpal pressure on dentin permeability and adhesion of self-etch adhesives. Dent Mater. 2006;
- Micropermeability of current self-etching and etch-and-rinse adhesives bonded to deep dentine: a comparison study using a double-staining/confocal microscopy technique. Eur J Oral Sci. 2008;116:184–193
- Application of hydrophobic resin adhesives to acid-etched dentin with an alternative wet bonding technique. J Biomed Mater Res A. 2008;84:19–29
- . Effects of resin hydrophilicity on dentin bond strength. J Dent Res. 2006;85(11):1016–1021
- Bonding BisGMA to dentin—a proof of concept for hydrophobic dentin bonding. J Dent Res. 2007;86:1034–1039
- . Tubular occlusion optimizes bonding of hydrophobic resins to dentin. J Dent Res. 2007;86:524–528
- Degree of conversion of resin blends in relation to ethanol content and hydrophilicity. Dent Mater. 2008;24:1194–1200
- . Two modes of nanoleakage expression in single-step adhesives. J Dent Res. 2002;81:472–476
- . Chemical–biological interactions of the resin monomer triethyleneglycol-dimethacrylate (TEGDMA). J Dent Res. 2001;80:2046–2050
- . Inhibition of phosphatidylinositol 3-kinase amplifies TEGDMA-induced apoptosis in primary human pulp cells. J Dent Res. 2004;83:703–707
- Pattern of cell death after in vitro exposure to GDMA, TEGDMA, HEMA and two compomer extracts. Dent Mater. 2006;22:630–640
- Adhesion to chondroitinase ABC treated dentin. J Biomed Mater Res B Appl Biomater. 2008;86:228–236
- . Hybridization efficiency of the adhesive/dentin interface with wet bonding. J Dent Res. 2003;82:141–145
- Collagen degradation by host-derived enzymes during aging. J Dent Res. 2004;83:216–221
- Micromorphological changes in resin–dentin bonds after one year of water storage. J Biomed Mater Res. 2002;63:306–311
- . Chlorhexidine arrests subclinical degradation of dentin hybrid layers in vivo. J Dent Res. 2005;84:741–746
- In vivo preservation of the hybrid layer by chlorhexidine. J Dent Res. 2007;86:529–533
- A critical review of the durability of adhesion to tooth tissue: methods and results. J Dent Res. 2005;84:118–132
- . Microtensile bond strength of a total-etch 3-step, total-etch 2-step, self-etch 2-step, and a self-etch 1-step dentin bonding system through 15-month water storage. J Adhes Dent. 2003;5:47–56
- . Adhesive phase separation at the dentin interface under wet bonding conditions. J Biomed Mater Res. 2002;62:447–456
- . The effect of chlorhexidine on dentin hybrid layers in vivo. Oper Dent. 2007;32:107–111
- Effect of 2% chlorhexidine digluconate on the bond strength to normal versus caries-affected dentin. Oper Dent. 2009;34:157–165
- Influence of chlorhexidine concentration on the durability of etch-and-rinse dentin bonds: a 12-month in vitro study. J Adhes Dent. 2009;11:191–198
- . Fatigue is more damaging than creep in ligament revealed by modulus reduction and residual strength. Ann Biomed Eng. 2007;35:1713–1721
PII: S0109-5641(09)00513-2
doi: 10.1016/j.dental.2009.12.009
© 2009 Academy of Dental Materials. Published by Elsevier Inc. All rights reserved.
« Previous
Next »
Dental Materials
Volume 26, Issue 4
, Pages 380-386
, April 2010