Dental Materials
Volume 25, Issue 8 , Pages 952-955, August 2009

Hertzian load-bearing capacity of a ceramic-reinforced glass ionomer cement stored wet and dry

  • Yan Wang

      Affiliations

    • Department of Prosthodontics, Guanghua School of Stomatology, Sun Yat-sen University, Guang Zhou, China
    • Dental Materials Science, Faculty of Dentistry, The University of Hong Kong, Hong Kong
  • ,
  • B.W. Darvell

      Affiliations

    • Dental Materials Science, Faculty of Dentistry, The University of Hong Kong, Hong Kong
    • Corresponding Author InformationCorresponding author at: Dental Materials Science, Prince Philip Dental Hospital, 34 Hospital Road, Hong Kong. Tel.: +852 2859 0303; fax: +852 2548 9464.

Received 6 March 2008; received in revised form 11 November 2008; accepted 12 February 2009.

To access this article, please choose from the options below

Login to an existing account or Register a new account.

  • Purchase this article for 31.50 USD (You must login/register to purchase this article)

    Online access for 24 hours. The PDF version can be downloaded as your permanent record.

  • Subscribe to this title

    Get unlimited online access to this article and all other articles in this title 24/7 for one year.

  • Claim access now

    For current subscribers with Society Membership or Account Number.

  • Visit SciVerse ScienceDirect to see if you have access via your institution.

PII: S0109-5641(09)00122-5

doi:10.1016/j.dental.2009.02.006

Dental Materials
Volume 25, Issue 8 , Pages 952-955, August 2009