SEM observations of porcelain Y-TZP interface
References
- . Haftverbundmechanismen in dentalen Schichtsystemen. Quintessenz Zahntechnik. 2007;33(2):160–168
- . An overview of zirconia ceramics: basic properties and clinical applications. J Dent. 2007;35(11):819–826
- . Phase transformation, roughness, and microhardness of artificially aged yttria- and magnesia-stabilized zirconia femoral heads. J Biomed Mater Res A. 2007;(June (21)):[Epub ahead of print]
- . Ceramics for prosthetic hip and knee joint replacement. J Am Ceram Soc. 2007;90(July (7)):1965–1988
- . Low-temperature degradation of zirconia and implications for biomedical implants. Annu Rev Mater Res. 2007;37:1–32
- . Long term in vivo and in vitro aging of a zirconia ceramic used in orthopaedy. J Biomed Mater Res. 1994;28:619–624
- Saint Gobain Desmarquest. Information on breakages reported on Prozyr-zirconia heads. http://www.prozyr.com/PAGESUK/Biomedical/figures.htm; 2004.
- . Five year clinical results of zirconia frameworks for posterior fixed partial dentures. Int J Prostodont. 2007;20(July–August (4)):383–388
- . Effect of thermal misfit between different veneering ceramics and zirconia frameworks on in vitro fracture load of single crowns. Dent Mater J. 2007;26(November (6)):766–772
- . All-ceramic FPDs made of DC-Zirkon—a clinical concept with success?. DZZ. 2005;60:435–445
- . Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing. Dent Mater. 2005;21:476–482
- Stephan M. Zur Entwicklung von ZrO2—Verstärkten Dentalkeramiken, Buch und Mensch Verlag, ISBN 3-89820-115-5, 2001.
- . Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia. J Biomed Mater Res. 1989;23(January (1)):45–61
- . Entwicklung der Metallkeramik. Zahnärztl Welt. 1980;89:36–41
- . Applied dental materials. 8th ed.. Blackwell Science; 1998;
- . New approach for evaluating metal–porcelain interfacial bonding. Int J Prosthodontics. 1999;12:547–552
- . Influence of the bonder on the adhesion of porcelain to machined titanium as determined by the strain energy release rate. Dent Mater. 2007;23(July (7)):822–828
- . Low-temperature aging of Y-TZP ceramics. J Am Ceram Soc. 1999;82:2150–2154
- . Determination of phase transformation depth profile with synchrotron radiation. J. Am. Ceram. Soc. 1987;70:227–231
- . Stability of Y-TZP during hydrothermal treatment: neutron experiments and stability considerations. J. Eur. Ceram. Soc. 2005;25:1597–1602
- Sangwal K. Etching of crystals: Theory, Experiment, and. Application. Amsterdam, Netherlands: North-Holland, 1987.