Dental Materials
Volume 25, Issue 4 , Pages 431-441 , April 2009

The development and testing of glaze materials for application to the fit surface of dental ceramic restorations

  • Michael J. Cattell

      Affiliations

    • Centre for Adult Oral Health, Barts and The London, School of Medicine and Dentistry, University of London, Turner Street, Whitechapel E1 2AD, UK
    • Corresponding Author InformationCorresponding author. Tel.: +44 2073777000x2160; fax: +44 2073777375.
  • ,
  • Thomas C. Chadwick

      Affiliations

    • 496 Alegre Avenue, Nipomo, CA 93444, USA
  • ,
  • Jonathan C. Knowles

      Affiliations

    • Division of Biomaterials and Tissue Engineering, Eastman Dental Institute, University College London, 256 Gray's Inn Road, London WC1X 8LD, UK
  • ,
  • Richard L. Clarke

      Affiliations

    • Department of Biomaterials in Relation to Dentistry, Francis Bancroft Building, Barts and The London, School of Medicine and Dentistry, University of London, Mile End Road, London E1 4NS, UK

Received 4 June 2008 ,Revised 22 August 2008 ,Accepted 25 September 2008.

References 

  1. Lawn B. In:  Davis EA,  Ward IM editor. Fracture in brittle solids. Cambridge: Cambridge University Press; 1993;p. 323–327
  2. Luthardt RG, Holzhuter MS, Rudolph H, Herold V, Walter MH. CAD/CAM-machining effects on Y-TZP zirconia. Dent Mater. 2004;20:655–662
  3. Binns DB. The chemical and physical properties of dental porcelain. In: McLean JW, editor. Dental ceramics, Proceedings of the 1st international symposium on dental ceramics. Quintessence Pub., Co., Chicago; 1983. p. 48–57.
  4. Beham G. IPS Empress; a new ceramic technology, Ivoclar-Vivadent Report. In: Dorsch P, editor. 1990;6:1–15.
  5. Addison O, Marquis PM, Fleming GJP. The impact of modifying alumina air abrasion parameters on the fracture strength of a porcelain laminate restorative material. Dent Mater. 2007;23:1332–1341
  6. Bhamra G, Palin WM, Fleming GJP. The effect of surface roughness on the flexure strength of an alumina reinforced all-ceramic crown material. J Dent. 2002;30:153–160
  7. Albakry M, Guazzato M, Swain MV. Effect of sandblasting, grinding, polishing and glazing on the flexural strength of two pressable all-ceramic dental materials. J Dent. 2004;32:91–99
  8. Creyke WEC. Delayed fracture of glazed porcelain. Trans J Br Ceram Soc. 1968;67:339–365
  9. Varshneya AK. Fundamentals of inorganic glasses. London: Academic Press Inc., Harcourt Brace and Co.; 1994;p. 445–8
  10. Brackett SE, Leary JM, Turner KA, Jordan RD. An evaluation of porcelain strength and the effect of surface treatment. J. Prosthet Dent. 1989;61:446–451
  11. Giordano R, Cima M, Prober R. The effect of surface finish on the flexural strength of feldspathic and aluminous dental ceramics. Int J Prosthodont. 1995;8:311–319
  12. Fairhurst CW, Lockwood PE, Dingle RD, Thompson WO. The effect of glaze on porcelain strength. Dent Mater. 1992;8:203–207
  13. Jones D, Wilson HJ. Some properties of dental porcelain. J Oral Rehabil. 1975;2:379–396
  14. Lüthy H, Dong JK, Wohlwend A, Schärer P. Effects of veneering and glazing on the strength of heat-pressed ceramics. Schweiz Monatsschr Zahnmed. 1993;10:1257–1260
  15. Wagner C, O’Brien WJ, Mora GP. Fracture-surface analysis of a glaze-strengthened magnesia core material. Int J Prosthodont. 1992;5:475–478
  16. Thompson JY, Anusavice KJ, Naman A, Morris HF. Fracture surface characterization of clinically failed all—ceramic crowns. J Dent Res. 1994;73:1824–1832
  17. Farah JW, Craig RG. Distribution of stresses in porcelain fused to metal and porcelain jacket crowns. J Dent Res. 1975;54:255–261
  18. Hillig WB, Charles RJ. Surfaces, stress dependent surface reactions and strength. In:  Zackay VF editors. High strength materials. New York: John Wiley and Sons Ltd.; 1965;p. 682–701
  19. Simonsen RJ, Calamia JR. Tensile bond strength of etched porcelain. J Dent Res. 1983;62:297;[Abstr. No. 1154]
  20. Van Noort R. Introduction to dental materials. London: Mosby; 1994;p. 61–71
  21. Calamia JR, Simonsen RJ. Effect of coupling agents on bond strength of etched porcelain. J Dent Res. 1984;63:179;[Abstr. No. 79]
  22. Stangel D, Natahson D, Hsu CS. Shear strength of the composite bond to etched porcelain. J Dent Res. 1987;66:1460–1465
  23. Nathanson D. Principles of porcelain use as an inlay/onlay material. In:  Garber DA,  Goldstein RE editor. Porcelain and composite inlays and onlays, esthetic posterior restorations. Carol Stream, Illinois: Quintessence Pub., Co., Inc.; 1994;p. 32–36
  24. Marquis PM. The influence of cements on the mechanical performance of dental ceramics. In: Proceedings of the fifth international symposium on ceramics in medicine. Bioceramics, vol. 5. Kobunshi Kankokai, Japan. 1992;p. 317–324
  25. Addison O, Marquis PM, Fleming GJP. Resin strengthening of dental ceramics—the impact of surface texture and silane. J Dent. 2007;35:416–424
  26. Fleming GJP, Maguire RF, Bhamra G, Burke FM, Marquis PM. The strengthening mechanism of resin cements on porcelain surfaces. J Dent Res. 2006;85:272–276
  27. Wassenaar P. The new porcelains—are they any better?. Aust Prosthodont J. 1990;4:19–25
  28. Lehner C, Studer S, Brodbeck U, Schärer P. Six-year clinical results of leucite-reinforced glass–ceramic inlays and onlays. Acta Med Dent Helv. 1998;3:137–146
  29. Studer S, Lehner C, Brodbeck U, Schärer P. Six-year results of leucite-reinforced glass–ceramic crowns. Acta Med Dent Helv. 1998;3:218–225
  30. Studer S, Lehner C, Schärer P. Seven-year results of results of leucite-reinforced glass–ceramic inlays and onlays. J Dent Res Spec Issue. 1998;77:802;[Abstr. No. 1375]
  31. Lehner C, Studer S, Scärer P. Seven year results of leucite reinforced glass ceramic crowns. J Dent Res Spec Issue. 1998;77:802;[Abstr. No. 1368]
  32. Cattell MJ, Chadwick TC, Knowles JC, Clarke RL, Lynch E. Flexural strength optimization of a leucite reinforced glass–ceramic. Dent Mater. 2001;17:21–33
  33. Thurmond JW, Barkmeier WW, Wilwerding TM. Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain. J Pros Dent. 1994;72:355–359
  34. Strassler HE. Minimally invasive porcelain veneers: indications for a conservative esthetic dentistry treatment modality. Gen Dent Spec Issue. 2007;55:686–694
  35. Jain P, Pershing A. Depth of cure and microleakage with high-intensity and ramped resin-based composite curing lights. J Am Dent Assoc. 2003;134:1215–1223
  36. Abernethey RB. The new Weibull handbook. 2nd ed.. Florida: Self published; 1996;p. 3.3–3.6
  37. James PF. Review: liquid-phase separation in glass-forming systems. J Mater Sci. 1975;10:1802–1825
  38. Zarzycki J. In:  Cahn RW,  Davies EA,  Ward IM editor. Glasses and the vitreous state. Cambridge Solid Science Series. Cambridge: Cambridge University Press; 1991;p. 164–226
  39. Ostwald W. Studen über die bildung und umwandlung fester körper. Z Phys Chem. 1897;22:289–330
  40. Vogel W, Gerth K. In:  Reser MK,  Smith GE,  Insley H editor. Symposium on nucleation and crystallization of glasses and melts. Columbus, Ohio: American Ceramic Society; 1962;p. 11–22
  41. Weyl WA. The constitution of glass. Coloured glasses.. Society of Glass Technology, Richard Clay and Co., Ltd.; 1951;p. 41–3
  42. McMillan PW. Glass–ceramics. 2nd ed.. London: Academic Press Inc.; 1979;p. 34–122
  43. Beall GH, Duke DA. Transparent glass ceramics. J Mater Sci. 1969;4:340–3352
  44. Hares GB, Morse DL. Method of producing a composite body United States Patent 4,683,168; 1987.
  45. Seward TP, Uhlmann DR, Turnbull D. Development of two-phase structures in glasses with special reference to the system BaO–SiO2. J Am Ceram Soc. 1968;51:634–643
  46. Simmons JH, Macedo PB, Napolitano A, Haller WK. Investigation of liquid–liquid phase transitions in oxide melts by viscosity measurements. Trans Faraday Soc. 1970;50:155–165
  47. Klaus I, Herbstman W, Lopez J. Dental compositions, fired dental porcelains and processes for making and using same. United States Patent 4,604,059; 1986.
  48. Della Bona A, Anusavice KJ. Microstructure, composition, and etching topography of dental ceramics. Int J Prosthodont. 2002;15:159–167
  49. Della Bona A, Shen C, Anusavice KJ. Work of adhesion of resin on treated lithia disilicate-based ceramic. Dent Mater. 2004;20:338–344
  50. Lacy AM, Laluz J, Watanabe LG, Dellinges M. Effect of porcelain surface treatment on the bond to composite. J Pros Dent. 1988;60:288–291
  51. Lu R, Harcourt JK, Tyas MJ, Alexander B. An investigation of the composite resin/porcelain interface. Aust Dent J. 1992;37:12–19
  52. Peumans M, Van Meerbeek B, Lambrechts P, Vanherle G. Porcelain veneers: a review of the literature. J Dent. 2000;28:163–177
  53. Chen JH, Matsumura H, Atsuta M. Effect of etchant, etching period, and silane priming on bond strength to porcelain of composite resin. Oper Dent. 1998;23:250–257
  54. Della Bona A. Characterizing ceramics and the interfacial adhesion to resin: II. The relationship of surface treatment, bond strength, interfacial toughness and fractography. J Appl Oral Sci. 2005;13:101–109
  55. Della Bona A, Van Noort R. Shear vs. tensile bond strength of resin composite bonded to ceramic. J Dent Res. 1995;74:1591–1596
  56. Oilo G. Bond strength testing: what does it mean?. Int Dent J. 1993;43:492–498
  57. Anderson GP, DeVries KL, Sharon G. Evaluation of tensile tests for adhesive bonds. In:  Johnson WS editors. Delamination and debonding of materials. Philadelphia: American Society for Testing and Materials special technical pub. 876; 1985;p. 115–134
  58. Dündar M, Özcan M, Gökçe B, Çömlekoğlu E, Leite F, Valandro LF. Comparison of two bond strength testing methodologies for bilayered all-ceramics. Dent Mater. 2007;23:630–636
  59. Addison O, Marquis PM, Fleming GJP. The impact of hydrofluoric acid surface treatments on the performance of a porcelain laminate restorative material. Dent Mater. 2007;23:461–468
  60. Walker MP, Spencer P, Eick JD. Mechanical property characterization of resin cement after aqueous aging with and without cyclic loading. Dent Mater. 2003;19:645–652
  61. Kern M, Wegner SM. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater. 1998;14:64–71
  62. Wang H, Aboushelib MN, Feilzer AJ. Strength influencing variables on CAD/CAM zirconia frameworks. Dent Mater. 2008;24:633–638
  63. Pitts PG, Vinson JR. Aerosolized ceramic porcelains and glaze composition. United States Patent 7,018,465; 2006.

PII: S0109-5641(08)00236-4

doi: 10.1016/j.dental.2008.09.004