Volume 24, Issue 10 , Pages 1352-1361 , October 2008

Fracture frequency of all-ceramic crowns during dynamic loading in a chewing simulator using different loading and luting protocols

  • S.D. Heintze

      Affiliations

    • R&D, Ivoclar Vivadent AG, Bendererstrasse 2, FL-9494 Schaan, Liechtenstein
    • Corresponding Author InformationCorresponding author. Tel.: +423 235 3570; fax: +423 233 1279.
  • ,
  • A. Cavalleri

      Affiliations

    • R&D, Ivoclar Vivadent AG, Bendererstrasse 2, FL-9494 Schaan, Liechtenstein
  • ,
  • G. Zellweger

      Affiliations

    • R&D, Ivoclar Vivadent AG, Bendererstrasse 2, FL-9494 Schaan, Liechtenstein
  • ,
  • A. Büchler

      Affiliations

    • Murten, Switzerland
  • ,
  • G. Zappini

      Affiliations

    • R&D, Ivoclar Vivadent AG, Bendererstrasse 2, FL-9494 Schaan, Liechtenstein

Received 10 September 2007 ,Accepted 11 February 2008.

References 

  1. Blatz MB. Long-term clinical success of all-ceramic posterior restorations. Quintessence Int. 2002;33:415–426
  2. Manhart J, Chen H, Hamm G, Hickel R. Buonocore Memorial Lecture. Review of the clinical survival of direct and indirect restorations in posterior teeth of the permanent dentition. Oper Dent. 2004;29:481–508
  3. El-Mowafy O, Brochu JF. Longevity and clinical performance of IPS-Empress ceramic restorations—a literature review. J Can Dent Assoc. 2002;68:233–237
  4. Edelhoff D, Horstkemper T, Richter E-J, Spiekermann H, Yildirim M. Adhäsiv und konventionell befestigte Empress 1-Kronen. Dtsch Zahnärztl Z. 2000;55:326–330
  5. Lehner C, Studer S, Schärer P. Seven-year results of leucite-reinforced glass-ceramic crowns. J Dent Res (Spec Iss) 1998;77:Abstract 1368.
  6. Fradeani M, Redemagni M. An 11-year clinical evaluation of leucite-reinforced glass-ceramic crowns: a retrospective study. Quintessence Int. 2002;33:503–510
  7. Gemalmaz D, Ergin S. Clinical evaluation of all-ceramic crowns. J Prosthet Dent. 2002;87:189–196
  8. Marquardt P, Strub JR. Survival rates of IPS Empress 2 all-ceramic crowns and fixed partial dentures: results of a 5-year prospective clinical study. Quintessence Int. 2006;37:253–259
  9. Behr M, Hindelang U, Rosentritt M, Lang R, Handel G. Comparison of failure rates of adhesive-fixed partial dentures for in vivo and in vitro studies. Clin Oral Investig. 2000;4:25–30
  10. Attia A, Kern M. Influence of cyclic loading and luting agents on the fracture load of two all-ceramic crown systems. J Prosthet Dent. 2004;92:551–556
  11. Strub JR, Beschnidt SM. Fracture strength of 5 different all-ceramic crown systems. Int J Prosthodont. 1998;11:602–609
  12. Malament KA, Grossman DG. Bonded vs. non bonded Dicor crowns: Four years report. J Dent Res (Spec Iss) 1992;71:Abstract 1720.
  13. Malament KA, Socransky SS, Thompson V, Rekow D. Survival of glass-ceramic materials and involved clinical risk: variables affecting long-term survival. Pract Proced Aesthet Dent. 2003;(Suppl.):5–11
  14. Sorensen JA, Choi C, Fanuscu MI, Mito WT. IPS Empress crown system: three-year clinical trial results. J Calif Dent Assoc. 1998;26:130–136
  15. Kelly JR. Clinically relevant approach to failure testing of all-ceramic restorations. J Prosthet Dent. 1999;81:652–661
  16. Rosentritt M, Behr M, Gebhard R, Handel G. Influence of stress simulation parameters on the fracture strength of all-ceramic fixed-partial dentures. Dent Mater. 2006;22:176–182[Epub 2005 Jul 21]
  17. Stappert CF, Att W, Gerds T, Strub JR. Fracture resistance of different partial-coverage ceramic molar restorations: An in vitro investigation. J Am Dent Assoc. 2006;137:514–522
  18. Krejci I, Lutz F. In-Vitro-Testverfahren zur Evaluation dentaler Restaurationssysteme Korrelation mit In-vivo-Resultaten. Schweiz Monatsschr Zahnmed. 1990;100:1445–1449
  19. Kelly JR. Ceramics in restorative and prosthetic dentistry. Annu Rev Mater Sci. 1997;27:443–468
  20. Rekow ED, Harsono M, Janal M, Thompson VP, Zhang G. Factorial analysis of variables influencing stress in all-ceramic crowns. Dent Mater. 2006;22:125–132[Epub 2005 Jul 5]
  21. Sobrinho LC, Cattell MJ, Glover RH, Knowles JC. Investigation of the dry and wet fatigue properties of three all-ceramic crown systems. Int J Prosthodont. 1998;11:255–262
  22. Scherrer SS, de Rijk WG. The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli. Int J Prosthodont. 1993;6:462–467
  23. Lee SK, Wilson PR. Fracture strength of all-ceramic crowns with varying core elastic moduli. Aust Dent J. 2000;45:103–107
  24. Schindler HJ, Stengel E, Spiess WE. Feedback control during mastication of solid food textures—a clinical-experimental study. J Prosthet Dent. 1998;80:330–336
  25. Kohyama K, Hatakeyama E, Sasaki T, Azuma T, Karita K. Effect of sample thickness on bite force studied with a multiple-point sheet sensor. J Oral Rehabil. 2004;31:327–334
  26. Gibbs CH, Mahan PE, Lundeen HC, Brehnan K, Walsh EK, Holbrook WB. Occlusal forces during chewing and swallowing as measured by sound transmission. J Prosthet Dent. 1981;46:443–449
  27. Nishigawa K, Bando E, Nakano M. Quantitative study of bite force during sleep associated bruxism. J Oral Rehabil. 2001;28:485–491
  28. Kohyama K, Hatakeyama E, Sasaki T, Dan H, Azuma T, Karita K. Effects of sample hardness on human chewing force: a model study using silicone rubber. Arch Oral Biol. 2004;49:805–816
  29. DeLong R, Douglas WH. Development of an artificial oral environment for the testing of dental restoratives: bi-axial force and movement control. J Dent Res. 1983;62:32–36
  30. Zhang Y, Lawn BR, Malament KA, Van Thompson P, Rekow ED. Damage accumulation and fatigue life of particle-abraded ceramics. Int J Prosthodont. 2006;19:442–448
  31. Rosentritt M, Behr M, Handel G. Fixed partial dentures: all-ceramics, fibre-reinforced composites and experimental systems. J Oral Rehabil. 2003;30:873–877
  32. Eschbach S, Koutayas S, Kern M. Fracture strength of resin-bonded all-ceramic fixed partial dentures. J Dent Res 2005 (Spec Issue A):Abstract No. 430.
  33. Attia A, Abdelaziz KM, Freitag S, Kern M. Fracture load of composite resin and feldspathic all-ceramic CAD/CAM crowns. J Prosthet Dent. 2006;95:117–123
  34. Kelly JR, Giordano R, Pober R, Cima MJ. Fracture surface analysis of dental ceramics: clinically failed restorations. Int J Prosthodont. 1990;3:430–440
  35. Thompson JY, Anusavice KJ, Naman A, Morris HF. Fracture surface characterization of clinically failed all-ceramic crowns. J Dent Res. 1994;73:1824–1832
  36. Ivoclar-Vivadent (2004). IPS Empress—Scientific Documentation.
  37. Ivoclar-Vivadent (2007). IPS e.max Press—Scientific Documentation.

PII: S0109-5641(08)00061-4

doi: 10.1016/j.dental.2008.02.019

Dental Materials
Volume 24, Issue 10 , Pages 1352-1361 , October 2008