Dental Materials
Volume 24, Issue 10 , Pages 1311-1315, October 2008

Marginal and internal fit of metal-ceramic crowns fabricated with a new laser melting technology

  • Katrin Quante

      Affiliations

    • Private Dental Office, Cologne, Germany
  • ,
  • Klaus Ludwig

      Affiliations

    • Department of Prosthodontics, Propaedeutics and Dental Materials, Dental School, Christian-Albrechts University at Kiel, Germany
  • ,
  • Matthias Kern

      Affiliations

    • Department of Prosthodontics, Propaedeutics and Dental Materials, Dental School, Christian-Albrechts University at Kiel, Germany
    • Corresponding Author InformationCorresponding author at: Arnold-Heller-Straße 16, 24105 Kiel, Germany. Tel.: +49 431 5972874; fax: +49 431 5972860.

Received 14 December 2007; received in revised form 17 February 2008; accepted 18 February 2008.

Abstract 

Objectives

The purpose of this in vivo investigation was to evaluate the marginal and internal fit of metal-ceramic crowns fabricated with a new laser melting procedure (BEGO Medical, Bremen, Germany), and to investigate the influence of ceramic firing on the marginal and internal accuracy of these crowns.

Methods

After tooth preparation, impression taking using polyvinylsiloxane and model casting, each preparation was contact less scanned by strip-light-projection. The finishing line and the virtual construction of the metal coping were defined by means of a computer. Using CAD/CAM software the metal copings were produced by BEGO Medical (Germany). A base metal alloy (Wirobond C) and a precious alloy (BioPontoStar, both: BEGO Medical) were used in this study with 14 restorations each.

The internal and marginal accuracy of the specimens were examined using a silicone indicator paste (Fit Checker, GC, Japan). After setting, the silicone films were embedded in acrylic resin and sectioned four times. Each slice was photographed digitally at 60× magnification for marginal and at 15× magnification for occlusal adaptation, respectively. Using a light microscope the thickness of the silicone layer was measured at 10 reference points, a total of 3360 measurements. This procedure was repeated after the ceramic firing in the dental laboratory and after intraoral adjustment clinically.

Results

No statistically significant differences between the two alloys were found at any time. The mean marginal discrepancies ranged from 74 to 99μm for both alloys. The internal gaps ranged from 250 to 350μm. Ceramic firing increased the marginal discrepancies while the internal gaps decreased especially at occlusal surface. However, only in one case a slight statistically significance could be determined (p=0.046).

Significance

The results of this in vivo study show that crowns produced with laser melting technology exhibit a marginal and internal accuracy that is comparable to conventional production procedures.

Keywords: Laser melting technology, Marginal fit, Precision, Ceramic veneered crown, Marginal discrepancies, Internal fit

To access this article, please choose from the options below

Login to an existing account or Register a new account.

  • Purchase this article for 31.50 USD (You must login/register to purchase this article)

    Online access for 24 hours. The PDF version can be downloaded as your permanent record.

  • Subscribe to this title

    Get unlimited online access to this article and all other articles in this title 24/7 for one year.

  • Claim access now

    For current subscribers with Society Membership or Account Number.

  • Visit SciVerse ScienceDirect to see if you have access via your institution.
 

PII: S0109-5641(08)00047-X

doi:10.1016/j.dental.2008.02.011

Dental Materials
Volume 24, Issue 10 , Pages 1311-1315, October 2008