Fractographic analyses of zirconia-based fixed partial dentures
References
- . All-ceramic fixed partial dentures designed according to the DC-Zirkon (R) technique. A 2-year clinical study. J Oral Rehabil. 2005;32:180–187
- . Ceramics update. J Dent. 1997;25:91–95
- . Three-year clinical evaluation of In-Ceram® Zirconia posterior FPDs. Int J Prosthodont. 2004;17:35–38
- . Mechanical-properties and short-term in vivo evaluation of yttrium-oxide-partially-stabilized zirconia. J Biomed Mater Res. 1989;23:45–61
- . Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM). Int J Comput Dent. 2001;4:89–106
- . All-ceramic restorations by new direct ceramic machining process (DCM). J Dent Res. 1998;77:762;[abstract 1046]
- . High reliable zirconia bridges by direct ceramic machining process (DCM). J Dent Res. 1998;77:762;[abstract no. 1045]
- . Fatigue of zirconia under cyclic loading in water and its implications for the design of dental bridges. Dent Mater. 2007;23:106–114
- . Strength and reliability of four-unit all-ceramic posterior bridges. Dent Mater. 2005;21:930–937
- . Influence of connector design on fracture probability of ceramic fixed-partial dentures. J Dent Res. 2002;81:623–627
- . Effect of connector design on the fracture resistance of all-ceramic fixed partial dentures. J Prosthet Dent. 2002;87:536–542
- . Fracture surface analysis of clinically failed fixed partial dentures. J Dent Res. 2006;85:277–281
- . Failure of all-ceramic fixed partial dentures in-vitro and in vivo—analysis and modeling. J Dent Res. 1995;74:1253–1258
- . Subcritical crack growth behavior of Al2O3–glass dental composites. J Biomed Mater Res B. 2003;65B:233–238
- . Fracture of brittle solids. 2nd ed.. Cambridge: Cambridge University Press; 1993;p. 106–12
- . Subcritical crack growth in ceramics. In: Bradt RC, Hasselman DPH, Lange FF editor. Fracture mechanics of ceramics. New York, NY: Plenum Press; 1974;p. 613–646
- . Fractography of slow fracture in glass. In: Mecholsky JJ, Powell SR editor. Fractography of ceramic and metal failures. Washington, DC: American Society for Testing and Materials; 1984;p. 121–136
- . Fractographic analyses of three ceramic whole crown restoration failures. Dent Mater. 2005;21:920–929
- . Fractography—determining the sites of fracture initiation. Dent Mater. 1995;11:113–116
- . Standard Practice for Fractography and Characterization of Fracture Origins in Advanced Ceramics, ASTM Designation C1322-96a. 1999 annual book of ASTM standards. vol. 15.01. West Conshohocken, PA: American Society for Testing and Materials; 1999;
- . An empirical stress intensity factor equation for the surface crack. Eng Fract Mech. 1981;15:185–192
- . Fracture-mechanics principles. Dent Mater. 1995;11:111–112
- . Mechanics of materials. 3rd ed.. New York: McGraw-Hill; 2002;p. 209–30
- . Characterization of fracture surfaces of dental ceramics. J Dent Res. 1994;73:196–1196
- . Fracture-surface analysis of dental ceramics. J Prosthet Dent. 1989;62:536–541
- . Residual stresses in bilayer dental ceramics. Biomaterials. 2005;26:3235–3241
PII: S0109-5641(08)00002-X
doi: 10.1016/j.dental.2007.12.006
© 2008 Academy of Dental Materials. Published by Elsevier Inc. All rights reserved.
« Previous
Next »
Dental Materials
Volume 24, Issue 8
, Pages 1077-1082
, August 2008