Three-body-wear resistance of the experimental composites containing filler treated with hydrophobic silane coupling agents

  • Tomotaro Nihei

      Affiliations

    • Department of Oral Medicine, Kanagawa Dental College, 82 Inaoaka-cho, Yokosuka, Kanagawa 238-8580, Japan
  • ,
  • Alp Dabanoglu

      Affiliations

    • Division of Restorative Dentistry, Dental School of Ludwig-Maximilians-University, Munich, Germany
  • ,
  • Toshio Teranaka

      Affiliations

    • Department of Oral Medicine, Kanagawa Dental College, 82 Inaoaka-cho, Yokosuka, Kanagawa 238-8580, Japan
    • Corresponding Author InformationCorresponding author. Tel.: +81 46 822 8854; fax: +81 46 822 8853.
  • ,
  • Shigeaki Kurata

      Affiliations

    • Department of Dental Materials and Devices, Kanagawa Dental College, Kanagawa, Japan
  • ,
  • Katsura Ohashi

      Affiliations

    • Department of Oral Medicine, Kanagawa Dental College, 82 Inaoaka-cho, Yokosuka, Kanagawa 238-8580, Japan
  • ,
  • Yukishige Kondo

      Affiliations

    • Department of Industrial Chemistry, Tokyo University of Science, Tokyo, Japan
  • ,
  • Norio Yoshino

      Affiliations

    • Department of Industrial Chemistry, Tokyo University of Science, Tokyo, Japan
  • ,
  • Reinhard Hickel

      Affiliations

    • Division of Restorative Dentistry, Dental School of Ludwig-Maximilians-University, Munich, Germany
  • ,
  • Karl-Heinz Kunzelmann

      Affiliations

    • Division of Restorative Dentistry, Dental School of Ludwig-Maximilians-University, Munich, Germany

Received 22 June 2007 ,Revised 25 August 2007 ,Accepted 11 September 2007.

References 

  1. Schrader ME, Block A. Tracer study of kinetics and mechanism of hydrolytically induced interfacial failure. J Polym Sci Part C. 1971;30:281–291
  2. Söderholm KJ. Degradation of glass filler in experiment composites. J Dent Res. 1981;60:1867–1875
  3. Söderholm KJ, Zigan M, Ragan M, Fischlschweiger W, Bergman M. Hydrolytic degradation of dental composites. J Dent Res. 1984;63:1248–1254
  4. Pillar RM, Smith DC, Maric B. Fracture toughness of dental composite determined using short-rod fracture toughness test. J Dent Res. 1986;65:1308–1314
  5. Calais JG, Söderholm KJ. Influence of filler type and water exposure on flexural strength of experimental composite resin. J Dent Res. 1988;67:836–840
  6. Ferracane JL, Marker VA. Solvent degradation and reduced fracture toughness in aged composite. J Dent Res. 1992;71:13–19
  7. Yamanaka H, Teranaka T, Kurata S, Yoshino N. Improvement of bond strength and water resistance of silane coupling agent containing poly(fluoro)alkyltrimethoxysilane. In: Joint Canada–Japan Workshop on Composites. Kyoto, Japan. 1996;p. 229–232
  8. Nihei T, Kurata S, Yamanaka H, Kurosaka N, Kondo Y, Yoshino N, et al. Improvement of long term water resistance of silane coupling agent layer modified with polyfluoroalkyltrimethoxysilane/3-methacryloyloxypropyl-trimethoxysilane mixture. Jpn J Dent Mater. 2000;19:495–501
  9. Nihei T, Kurata S, Kondo Y, Umemoto K, Yoshino N, Teranaka T. Enhanced hydrolytic stability of dental composites by use of fluoroalkyltrimethoxysilanes. J Dent Res. 2002;81:482–486
  10. Okada H, Kondo Y, Yoshino N. Synthesis of aromatic silane coupling agents having a polymerizable group. Mater Technol. 2001;19:197–202
  11. Nihei T, Kurata S, Ohashi K, Kondo Y, Umemoto K, Yoshino N, et al. Water resistance of novel silane coupling agents having aromatic group substituted a reactive double bond. Jpn J Dent Mater. 2005;24:1–8
  12. Ohashi K, Nihei T, Kurata S, Kondo Y, Umemoto K, Yoshino N, et al. Adhesion of resin to ceramic surface modified with phenyl group silane coupling agents containing a double bond. Jpn J Dent Mater. 2005;24:247–252
  13. Mehl A, Gloger W, Kunzelmann KH, Hickel R. A new optical 3D device for the detection of wear. J Dent Res. 1997;76:1799–1807
  14. Oysaed H, Ruyter IE. Composites for use in posterior teeth: mechanical properties under dry and wet conditions. J Biomed Mater Res. 1986;20:261–271
  15. Montes-G GM, Draughn RA. In vitro surface degradation of composites by wear and thermal cycling. Dent Mater. 1986;2:193–197
  16. Frazier KB, Sarrett DC. Wear resistance of dual-cures resin luting agents. Am J Dent. 1995;8:161–164
  17. Venhowen BMA, De Gee AJ, Werner A, Davidson CL. Influence of filler parameters on the mechanical adherence of dental restorative resin composites. Biomaterials. 1996;17:735–740
  18. Söderholm KJ, Richards ND. Wear resistance of composites: a solved problem?. Gen Dent. 1998;46:256–264
  19. De Gee AJ, Pallaw P. Occlusal wear simulation with ACTA wear machine. J Dent. 1994;22(Suppl 1):S21–S27
  20. Mair LH, Stolarski TA, Vowles RW, Lloyd CH. Wear: mechanisms, manifestations and measurement. Report of a workshop. J Dent. 1996;24:141–148
  21. Lutz F, Phillips RW, Roulet JF, Setcos JC. In vivo and in vitro wear of potential posterior composites. J Dent Res. 1984;63:914–920
  22. Embong A, Glyn Jones J, Harrison A. The wear effects of selected composites on restorative materials and enamel. Dent Mater. 1987;3:236–240
  23. Gallegos LI, Nicholls JI. In vitro two-body wear of three veneering resins. J Prosthet Dent. 1988;60:172–178
  24. Leinfelder KF, Beaudreau RW, Mazer RB. An in vitro device for predicting clinical wear. Quint Int. 1989;20:755–761
  25. Sarrett DC, Söderholm KJ, Batich CD. Water and abrasive effect on three-body wear of composites. J Dent Res. 1991;70:1074–1081
  26. Graf K, Johnson GH, Mehl A, Rammelsberg P. The influence of dental alloys on three-body wear of human enamel and dentin in an inlay-like situation. Oper Dent. 2002;27:167–174
  27. Sunnegardh-Gronberg K, Peutzfeldt A, van Dijken JW. Hardness and in vitro wear of a novel ceramic restorative cement. Eur J Oral Sci. 2002;110:175–178
  28. Say EC, Civelek A, Nobecourt A, Ersoy M, Guleryuz C. Wear and microhardness of different resin composite materials. Oper Dent. 2003;28:628–634
  29. Kunzelmann KH, Bürkle V, Bauer C. Two-body and three-body wear of glass ionomer cements. Int J Paediatr Dent. 2003;13:434–440
  30. Schwartz JI, Söderholm KJ. Effect of filler size, water, and alcohol on hardness and laboratory wear of dental composites. Acta Odontol Scand. 2004;62:102–106
  31. Arikawa H, Kuwahata H, Seki H, Kanie T, Fujii K, Inoue K. Deterioration of mechanical properties of composite resin. Dent Mater J. 1995;14:78–83
  32. Kurata S, Yamazaki N. Effect of silane coupling agents with various organofunctional and hydrolyzable group on silicon and its water-resistance. Jpn J Dent Mater. 1992;11:916–921
  33. Teranaka T, Iwamoto T, Yoshino N. Application of newly developed surface modifier to dental material. Bull Kanagawa Dent Coll. 1994;22:151–155
  34. Plueddemann EP, Pape PG. The use of mixed silane coupling agents. In: Proceedings of the 40th Annual Conference, Reinforced Plastics/Composites Institute, Session 17-F. The Society of the Plastics Industry Inc.; 1985;p. 1–4
  35. Karata S, Yamazaki N. Effect of silane coupling agents with a bisfunctional hydrolyzable group. Dent Mater J. 1993;12:127–135
  36. Craig RG, Dootz ER. Effect of mixed silanes on the hydrolytic stability of composites. J Oral Rehabil. 1996;23:751–756
  37. Morikawa A, Iyoku Y, Kakimoto M, Imai Y. Preparation on new polyimide-silica hybrid materials via the sol–gel process. J Mater Chem. 1992;2:679–690

PII: S0109-5641(07)00219-9

doi: 10.1016/j.dental.2007.09.001

Dental Materials
Volume 24, Issue 6 , Pages 760-764 , June 2008