Dental Materials
Volume 24, Issue 5 , Pages 618-622, May 2008

Influence of preparation of ceramic SEVNB specimens on fracture toughness testing results

Department of Ceramics and Refractory Materials, Institute of Mineral Engineering, RWTH Aachen University, Mauerstrasse 5, D-52064 Aachen, Germany

Received 9 November 2006; accepted 25 June 2007.

To access this article, please choose from the options below

Login to an existing account or Register a new account.

  • Purchase this article for 31.50 USD (You must login/register to purchase this article)

    Online access for 24 hours. The PDF version can be downloaded as your permanent record.

  • Subscribe to this title

    Get unlimited online access to this article and all other articles in this title 24/7 for one year.

  • Claim access now

    For current subscribers with Society Membership or Account Number.

  • Visit SciVerse ScienceDirect to see if you have access via your institution.

PII: S0109-5641(07)00164-9

doi:10.1016/j.dental.2007.06.021

Dental Materials
Volume 24, Issue 5 , Pages 618-622, May 2008