Dental Materials
Volume 23, Issue 11 , Pages 1397-1404 , November 2007

Fractographic ceramic failure analysis using the replica technique

  • Susanne S. Scherrer

      Affiliations

    • Department of Prosthodontics-Biomaterials, University of Geneva, School of Dental Medicine, 19, Barthélemy-Menn, 1205 Geneva, Switzerland
    • Corresponding Author InformationCorresponding author. Tel.: +41 22 3794069; fax: +41 22 3794052.
  • ,
  • Janet B. Quinn

      Affiliations

    • American Dental Association Foundation-PRC, National Institute of Standards and Technology, Gaithersburg, MD, USA
  • ,
  • George D. Quinn

      Affiliations

    • National Institute of Standards and Technology, Ceramics Division, Gaithersburg, MD, USA
  • ,
  • H.W. Anselm Wiskott

      Affiliations

    • Department of Prosthodontics-Biomaterials, University of Geneva, School of Dental Medicine, 19, Barthélemy-Menn, 1205 Geneva, Switzerland

Received 16 June 2006 ,Accepted 6 December 2006.

References 

  1. Kelly JR, Campbell SD, Bowen HK. Fracture-surface analysis of dental ceramics. J Prosthet Dent. 1989;62:536–541
  2. Kelly JR, Giordano R, Pober R, Cima MJ. Fracture-surface analysis of dental ceramics: clinically failed restorations. Int J Prosthodont. 1990;3:430–440
  3. Thompson JY, Anusavice KJ, Morris H. Fracture surface characterization of clinically failed all-ceramic crowns. J Dent Res. 1994;73:1824–1832
  4. Kelly JR. Fractography of dental ceramics. In:  Varner JR,  Quinn GD editor. Fractography of glasses and ceramics IV. vol. 122:Westerville, OH: American Ceramic Society; Ceramic Transactions; 2001;p. 241–251
  5. Quinn JB, Quinn GD, Kelly JR, Scherrer SS. Fractographic analyses of three ceramic whole crown restoration failures. Dent Mater. 2005;21:920–929
  6. Taskonak B, Mecholsky JJ, Anusavice KJ. Fracture surface analysis of clinically failed fixed partial dentures. J Dent Res. 2006;85:277–281
  7. Scherrer SS, Quinn JB, Quinn GD, Kelly JR. Failure analysis of ceramic clinical cases using qualitative fractography. Int J Prosthodont. 2006;19:151–158
  8. Rice RW. Ceramic fracture features, observations, mechanisms and uses. In:  Mecholsky JJ,  Powel SR editor. Fractography of ceramics and metal failures, ASTM STP 827. Philadelphia: American Society for Testing and Materials; 1984;p. 5–103
  9. Fréchette VD. Failure analysis of brittle materials. Advances in ceramics. vol. 28. Westerville, OH: American Ceramic Society; 1990;
  10. Varner JR. Descriptive fractography. In:  Schneider SJ editors. Ceramics and glasses, engineered materials handbook. vol. 4:Metals Park, Ohio: ASM International; 1991;p. 635–644
  11. Quinn GD. Recommended practice guide for fractography of ceramics and glasses. Gaithersburg, MD: National Institute of Standards and Technology; 2006;Special Publication 960-XX
  12. ASTM C1322-05a. Standard practice for fractography and characterization of fracture origins in advanced ceramics. West Conshohoken, PA: ASTM International; 2005;

PII: S0109-5641(06)00325-3

doi: 10.1016/j.dental.2006.12.002

Dental Materials
Volume 23, Issue 11 , Pages 1397-1404 , November 2007