Volume 23, Issue 11 , Pages 1382-1389 , November 2007

Wear of composite resin veneering materials and enamel in a chewing simulator

  • Christian Mehl

      Affiliations

    • Department of Prosthodontics, Propaedeutics and Dental Materials, Dental School, Christian-Albrechts-University at Kiel, Germany
  • ,
  • Soeren Scheibner

      Affiliations

    • Private Practice, Neuburg, Germany
  • ,
  • Klaus Ludwig

      Affiliations

    • Department of Prosthodontics, Propaedeutics and Dental Materials, Dental School, Christian-Albrechts-University at Kiel, Germany
  • ,
  • Matthias Kern

      Affiliations

    • Department of Prosthodontics, Propaedeutics and Dental Materials, Dental School, Christian-Albrechts-University at Kiel, Germany
    • Corresponding Author InformationCorresponding author at: Arnold-Heller-Strasse 16, 24105 Kiel, Germany. Tel.: +49 431 5972874; fax: +49 431 5972860.

Received 10 May 2006 ,Revised 18 November 2006 ,Accepted 21 November 2006.

References 

  1. Willems G, Lambrechts P, Braem M, Vanherle G. Composite resins in the 21st century. Quintessence Int. 1993;24:641–658
  2. Mair LH. Wear in dentistry–current terminology. J Dent. 1992;20:140–144
  3. Powers JM, Allen LJ, Craig RG. Two-body abrasion of commercial and experimental restorative and coating resins and an amalgam. J Am Dent Assoc. 1974;89:1118–1122
  4. Harrison A, Lewis TT. The development of an abrasion testing machine for dental materials. J Biomed Mater Res. 1975;9:341–353
  5. McCabe JF, Smith BH. A method for measuring the wear of restorative materials in vitro. Br Dent J. 1981;151:123–126
  6. Lutz F, Phillips RW, Roulet JF, Setcos JC. In vivo and in vitro wear of potential posterior composites. J Dent Res. 1984;63:914–920
  7. De Gee AJ, Pallav P, Davidson CL. Effect of abrasion medium on wear of stress-bearing composites and amalgam in vitro. J Dent Res. 1986;65:654–658
  8. Marquis PM, Hu X, Shortall AC. Two-body wear of dental composites under different loads. Int J Prosthodont. 2000;13:473–479
  9. 14569-2 IT. Dental materials—Guidance on testing of wear.Part 2. Wear by two- and or three-body contact.
  10. DeLong R, Douglas WH. Development of an artificial oral environment for the testing of dental restoratives: bi-axial force and movement control. J Dent Res. 1983;62:32–36
  11. de Gee AJ, Pallav P. Occlusal wear simulation with the ACTA wear machine. J Dent. 1994;22(Suppl. 1):S21–S27
  12. Cha HS, Lee YK, Lim BS, Rhee SH, Yang HC. Evaluation of wear resistance of dental resin composites with a 3D profilometer. J Biomed Mater Res B Appl Biomater. 2004;71:414–420
  13. DeLong R, Pintado M, Douglas WH. Measurement of change in surface contour by computer graphics. Dent Mater. 1985;1:27–30
  14. Sakaguchi RL, Douglas WH, DeLong R, Pintado MR. The wear of a posterior composite in an artificial mouth: a clinical correlation. Dent Mater. 1986;2:235–240
  15. Krejci I, Heinzmann JL, Lutz F. The wear on enamel, amalgam and their enamel antagonists in a computer-controlled mastication simulator. Schweiz Monatsschr Zahnmed. 1990;100:1285–1291
  16. Kern M, Strub JR, Lu XY. Wear of composite resin veneering materials in a dual-axis chewing simulator. J Oral Rehabil. 1999;26:372–378
  17. Wassell RW, McCabe JF, Walls AW. Wear characteristics in a two-body wear test. Dent Mater. 1994;10:269–274
  18. Wassell RW, McCabe JF, Walls AW. A two-body frictional wear test. J Dent Res. 1994;73:1546–1553
  19. Krejci I, Lutz F, Gautschi L. Wear and marginal adaptation of composite resin inlays. J Prosthet Dent. 1994;72:233–244
  20. Krejci I, Mueller E, Lutz F. Effects of thermocycling and occlusal force on adhesive composite crowns. J Dent Res. 1994;73:1228–1232
  21. Heintze SD, Cavalleri A, Forjanic M, Zellweger G, Rousson V. A comparison of three different methods for the quantification of the in vitro wear of dental materials. Dent Mater. 2006;22:1051–1062
  22. In:  Siegel J editors. Statistix Version 4 User's Manual. St. Paul: Analytical Software; 1992;
  23. Hu X, Marquis PM, Shortall AC. Influence of filler loading on the two-body wear of a dental composite. J Oral Rehabil. 2003;30:729–737
  24. Knobloch LA, Kerby RE, Seghi R, van Putten M. Two-body wear resistance and degree of conversion of laboratory-processed composite materials. Int J Prosthodont. 1999;12:432–438
  25. Frankenberger R, Garcia-Godoy F, Lohbauer U, Petschelt A, Kramer N. Evaluation of resin composite materials. Part I: in vitro investigations. Am J Dent. 2005;18:23–27
  26. Reich SM, Petschelt A, Wichmann M, Frankenberger R. Mechanical properties and three-body wear of veneering composites and their matrices. J Biomed Mater Res A. 2004;69:65–69
  27. Mair LH, Stolarski TA, Vowles RW, Lloyd CH. Wear: mechanisms, manifestations and measurement. Report of a workshop. J Dent. 1996;24:141–148
  28. Xu HH, Quinn JB, Giuseppetti AA, Eichmiller FC, Parry EE, Schumacher GE. Three-body wear of dental resin composites reinforced with silica-fused whiskers. Dent Mater. 2004;20:220–227
  29. Krejci I, Albert P, Lutz F. The influence of antagonist standardization on wear. J Dent Res. 1999;78:713–719
  30. Shortall AC, Hu XQ, Marquis PM. Potential countersample materials for in vitro simulation wear testing. Dent Mater. 2002;18:246–254
  31. Kielbassa AM, Gillmann L, Zantner C, Meyer-Lueckel H, Hellwig E, Schulte-Monting J. Profilometric and microradiographic studies on the effects of toothpaste and acidic gel abrasivity on sound and demineralized bovine dental enamel. Caries Res. 2005;39:380–386
  32. Turssi CP, Messias DC, de Menezes M, Hara AT, Serra MC. Role of dentifrices on abrasion of enamel exposed to an acidic drink. Am J Dent. 2005;18:251–255
  33. Suzuki S, Nagai E, Taira Y, Minesaki Y. In vitro wear of indirect composite restoratives. J Prosthet Dent. 2002;88:431–436
  34. Heintze SD, Zappini G, Rousson V. Wear of ten dental restorative materials in five wear simulators–results of a round robin test. Dent Mater. 2005;21:304–317
  35. Gegauff AG, Garcia JL, Koelling KW, Seghi RR. Thermoplastic composites for veneering posterior teeth-a feasibility study. Dent Mater. 2002;18:479–485
  36. Lim BS, Ferracane JL, Condon JR, Adey JD. Effect of filler fraction and filler surface treatment on wear of microfilled composites. Dent Mater. 2002;18:1–11
  37. Turssi CP, Ferracane JL, Vogel K. Filler features and their effects on wear and degree of conversion of particulate dental resin composites. Biomaterials. 2005;26:4932–4937
  38. Mandikos MN, McGivney GP, Davis E, Bush PJ, Carter JM. A comparison of the wear resistance and hardness of indirect composite resins. J Prosthet Dent. 2001;85:386–395

PII: S0109-5641(06)00315-0

doi: 10.1016/j.dental.2006.11.026

Dental Materials
Volume 23, Issue 11 , Pages 1382-1389 , November 2007