Dental Materials
Volume 23, Issue 11 , Pages 1356-1362 , November 2007

Short glass fiber reinforced restorative composite resin with semi-inter penetrating polymer network matrix

Received 4 July 2006 ,Accepted 16 November 2006.

References 

  1. Bowen RL. Properties of a silica-reinforced polymer for dental restorations. J Am Dent Assoc. 1963;66:57–64
  2. Wilder AD, May KN, Bayne SC, Taylor DF, Leinfelder KF. Seventeen-year clinical study of ultraviolet-cured posterior composite Class I and II restorations. J Esthet Dent. 1999;11:135–142
  3. Opdam NJ, Loomans BA, Roeters FJ, Bronkhorst EM. Five-year clinical performance of posterior resin composite restorations placed by dental students. J Dent. 2004;32:379–383
  4. Roulet JF. Benefits and disadvantages of tooth-coloured alternatives to amalgam. J Dent. 1997;25:459–473
  5. Manhart J, Chen H, Hamm G, Hickel R, Buonocore . Memorial Lecture. Review of the clinical survival of direct and indirect restorations in posterior teeth of the permanent dentition. Oper Dent. 2004;29:481–508
  6. Ferracane JL, Berge HX, Condon JR. In vitro aging of dental composites in water—effect of degree of conversion, filler volume, and filler/matrix coupling. J Biomed Mater Res. 1998;42:465–472
  7. Asmussen E. Restorative resins: hardness and strength vs. quantity of remaining double bonds. Scand J Dent Res. 1982;90:484–489
  8. Eick JD, Kaufman GM, Chappelow CC. Applications of polymers: what are the future trend?. Acad Dent Mater Trans. 1979;10:89–98
  9. Watts DC, Hindi AA. Intrinsic soft-start polymerization shrinkage-kinetics in an acrylate-based resin composite. Dent Mater. 1999;15:39–45
  10. Krause WR, Park SH, Straup RA. Mechanical properties of Bis-GMA resin short glass fiber composites. J Biomed Mater Res. 1998;23:1195–1211
  11. Petersen RC. Discontinuous fiber-reinforced composites above critical length. J Dent Res. 2005;84:365–370
  12. Bayne SC, Thompson JY. Mechanical property analysis of two admixed PRIMM-modified commercial dental composites. Trans Acad Dent Mater. 1996;9:238
  13. Garoushi S, Lassila LVJ, Tezvergil A, Vallittu PK. Load bearing capacity of fiber-reinforced and particulate filler composite resin combination. J Dent. 2006;34:179–184
  14. Xu HHK, Quinn JB, Smith DT, Giuseppetti AA, Eichmiller FC. Effect of different whiskers on the reinforcement of dental resin composites. Dent Mater. 2003;19:359–367
  15. Zandinejad AA, Atai M, Pahlevan A. The effect of ceramic and porous fillers on the mechanical properties of experimental dental composites. Dent Mater. 2006;22:382–387
  16. Loza-Herrero MA, Rueggeberg FA, Caughman WF, Schuster GS, Lefebvre CA, Gardner FM. Effect of heating delay on conversion and strength of a post-cured resin composite. J Dent Res. 1998;77:426–431
  17. Xu HH. Dental composite resins containing silica-fused ceramic single-crystalline whiskers with various filler levels. J Dent Res. 1999;78:1304–1311
  18. Wilder AD, Bayne SC, Heymann HO. Long-term clinical performance of direct posterior composites. Trans Acad Dent Mater. 1996;9:151–169
  19. Vallittu PK. A review of fiber-reinforced denture base resins. J Prosthodont. 1996;5:270–276
  20. Vallittu PK. Comparison of the in vitro fatigue resistance of acrylic resin removable partial denture reinforced with continuous glass fibers or metal wires. J Prosthodont. 1996;5:115–121
  21. Vallittu PK. Comparison of two different silane compounds used for improving adhesion between fibers and acrylic denture base material. J Oral Rehabil. 1993;20:533–539
  22. Vallittu PK, Narva K. Impact strength of a modified continuous glass fiber-poly(methyl methacrylate). Int J Prosthodont. 1997;10:142–148
  23. Vallittu PK, Lassila VP, Lappalainen R. Acrylic resin-fiber composite. Part I: The effect of fiber concentration on fracture resistance. J Prosthet Dent. 1994;71:607–612
  24. Stipho HD. Repair of acrylic resin denture base reinforced with glass fiber. J Prosthet Dent. 1998;80:546–550
  25. Ladizesky NH, Cheng YY, Chow TW, Ward IM. Acrylic resin reinforced with chopped high performance polyethylene fiber properties and denture construction. Dent Mater. 1993;9:128–135
  26. Dyer SR, Lassila LVJ, Jokinen M, Vallittu PK. Effect of fiber position and orientation on fracture load of fiber reinforced composite. Dent Mater. 2004;20:947–955
  27. Vallittu PK. The effect of void space and polymerization time on transverse strength of acrylic-glass fiber composite. J Oral Rehabil. 1995;22:257–261
  28. Miettinen VM, Vallittu PK. Water sorption and solubility of glass fiber-reinforced denture polymethyl methacrylate. J Prosthet Dent. 1997;77:531–534
  29. Vishu S. Handbook of plastic testing technology. 2nd ed.. New York: John Wiley; 1998;p. 546
  30. Lastumäki TM, Lassila LV, Vallittu PK. The semi-interpenetrating polymer network matrix of fiber-reinforced composite and its effect on the surface adhesive properties. J Mater Sci Mater Med. 2003;14:803–809
  31. Lassila LV, Tezvergil A, Lahdenpera M, Alander P, Shinya A, Vallittu PK. Evaluation of some properties of two fiber reinforced composite materials. Acta Odontol Scand. 2005;63:196–204
  32. Söderholm KJ, Yang MC, Garcea I. Filler particle leachability of experimental dental composites. Eur J Oral Sci. 2000;108:555–560
  33. International Standardization Organization, ISO 10477-1992(E). Polymer-based crown and bridge material. Geneva: ISO; 1992.
  34. Van Dijken JWV, Grönberg KS. Fibre-reinforced packable resin composite in Class II cavities. J Dent. 2006;34:763–769
  35. Nielsen LE. Mechanical properties of polymer and composites. New York: Marcel Dekker; 1974;
  36. Vallittu PK, Lassila VP, Lappalainen R. Transverse strength and fatigue of denture acrylic-glass fiber composite. Dent Mater. 1994;10:116–121
  37. Cheng TH, Jones FR, Wang D. Effect of fiber conditioning on the interfacial shear strength of glass-fiber composite. Compos Sci Technol. 1993;48:89–96
  38. Karacaer Ö, Polat TN, Tezvergil A, Lassila LVJ, Vallittu PK. The effect of length and concentration of glass fibers on the mechanical properties of an injection- and a compression-molded denture base polymer. J Prosthet Dent. 2003;90:385–393
  39. Vallittu PK. Flexural properties of acrylic resin polymers reinforced with unidirectional and woven glass fibers. J Prosthet Dent. 1999;81:318–326
  40. Alander P, Lassila LVJ, Vallittu P. The span length and cross-section design affect values of strength. Dent Mater. 2005;21:347–353
  41. Ferracane JL, Greener EH. Fourier transform infrared analysis of degree of polymerization in unfilled resins-method comparison. J Dent Res. 1984;63:1093–1095
  42. Halvorson RH, Erickson RL, Davidson CL. The effect of filler and silane content on conversion of resin-based composite. Dent Mater. 2003;19:327–333
  43. Vallittu PK, Ruyter IE, Ekstrand K. Effect of 180-week water storage on the flexural properties of E-glass and silica fiber acrylic resin composite. Int J Prosthodont. 2000;13:334–339
  44. Lassila LVJ, Nohrström T, Vallittu PK. The influence of short-term water storage on the flexural properties of unidirectional glass fiber-reinforced composites. Biomaterials. 2002;23:2221–2229
  45. Abdel-Magid B, Ziaee S, Gass K, Schneider M. The combined effects of load, moisture and temperature on the properties of E-glass/epoxy composites. Compos Struct. 2005;71:320–326
  46. Uno S, Shimokobe H. Contraction stress and marginal adaptation of composite restorations in dentinal cavity. Dent Mater J. 1994;13:19–24

PII: S0109-5641(06)00311-3

doi: 10.1016/j.dental.2006.11.017

Dental Materials
Volume 23, Issue 11 , Pages 1356-1362 , November 2007