The impact of hydrofluoric acid surface treatments on the performance of a porcelain laminate restorative material

  • Owen Addison

      Affiliations

    • Biomaterials Unit, University of Birmingham, School of Dentistry, St. Chad's Queensway, Birmingham B4 6NN, UK
    • Corresponding Author InformationCorresponding author at: Biomaterials Unit, University of Birmingham School of Dentistry, St. Chad's Queensway, Birmingham, UK. Tel.: +44 237 2911; fax: +44 237 2932.
  • ,
  • Peter M. Marquis

      Affiliations

    • Biomaterials Unit, University of Birmingham, School of Dentistry, St. Chad's Queensway, Birmingham B4 6NN, UK
  • ,
  • Garry J.P. Fleming

      Affiliations

    • Materials Science Unit, Division of Oral Biosciences, Dublin Dental School and Hospital, Trinity College Dublin, Dublin 2, Republic of Ireland

Received 16 November 2005 ,Revised 23 February 2006 ,Accepted 9 March 2006.

References 

  1. McLean JW. Ceramics in clinical dentistry. Br Dent J. 1988;164:187–194
  2. Burke FJT, Qualtrough AJE, Hale RW. Dentine-bonded all-ceramic crowns: current status. J Am Dent Assoc. 1998;129:455–460
  3. Lacy AM, Laluz J, Watanabe LG, Dellinges M. Effect of porcelain surface treatment on the bond to composite. J Prosthet Dent. 1995;60:288–291
  4. Horn HR. Porcelain laminate veneers bonded to etched enamel. In:  Phillips RW editors. Symposium on dental materials, vol. 27. Dental Clinics of North America. 1983;p. 671–684
  5. Wolf DM, Powers JM, O’Keefe KL. Bond strength of composite to etched and sandblasted porcelain. Am J Dent. 1993;6:155–158
  6. Stangel I, Nathanson D, Hsu CS. Shear strength of the composite bond to etched porcelain. J Dent Res. 1987;66:1460–1465
  7. Proctor B. The effects of hydrofluoric acid etching on the strength of glasses. Phys Chem Glass. 1962;3:7–27
  8. Magne P, Kwon KR, Besler C, Hodges JS, Douglas WH. Crack propensity of porcelain laminate veneers- a simulated operatory evaluation. J Prosthet Dent. 1999;81:327–334
  9. Yen T, Blackman RB, Baez RJ. Effect of acid etching on the flexural strength of a feldspathic porcelain and castable glass ceramic. J Prosthet Dent. 1993;70:224–233
  10. Mikeska KR, Bennison SJ, Grise SL. Corrosion of ceramics in aqueous hydrofluoric acid. J Am Ceram Soc. 2000;83:1160–1164
  11. Addison O, Fleming GJP. The influence of cement lute, thermocycling and surface preparation on the strength of a porcelain laminate veneering material. Dent Mater. 2004;20:286–292
  12. Kato H, Matsumura H, Atsuta M. Effect of etching and sandblasting on bond strength to sintered porcelain of unfilled resin. J Oral Rehabil. 2000;27:103–110
  13. Fleming GJP, Jandu HS, Nolan L, Shaini FJ. The influence of alumina abrasion and cement lute on the strength of a porcelain laminate veneering material. J Dent. 2004;32:67–74
  14. Della Bona A, Anusavice KJ. Microstructure, composition and etching topography of dental ceramics. Int J Prosthodont. 2002;15:159–167
  15. Fleming GJP, Shaini FJ, Marquis PM. An assessment of the influence of mixing induced variability on the bi-axial flexure strength of dentine porcelain discs and the implications for laboratory testing of porcelain specimens. Dent Mater. 2000;16:114–119
  16. Anusavice KJ, Lee RB. Effect of firing temperature and water exposure on crack propagation in unglazed porcelain. J Dent Res. 1989;68:1075–1081
  17. Timoshenko S, Woinowsky-Krieger S. Symmetrical bending of circular plates. Theory of plates and shells. 2nd ed.. New York: McGraw-Hill; 1959;p. 87–121
  18. Anusavice KJ, DeHoff PH, Fairhurst EW. Comparative evaluation of ceramic-metal bond tests using finite element analysis. J Dent Res. 1980;59:608–613
  19. Weibull W. A statistical distribution function of wide applicability. J Appl Mech. 1951;18:293–297
  20. Ritter JE, Bandyopadhyay N, Jakus K. Statistical reproducibility of the dynamic and static fatigue experiments. Ceram Bull. 1981;60:798–806
  21. Kobayashi K. Crystallized fused SiO2 glass strength improvement by etching. Phys Chem Glasses. 1962;3:7–27
  22. Baikova LG, Pukh VP, Pesina TI. Effect of chemical etching on the strength of undamaged glass. Soviet J Glass Phys Chem. 1983;9:452–456
  23. Coble RL, Parikh NM. Fracture in Polycrystalline Ceramics. In:  Liebowitz H editors. Fracture: and advanced treatise. New York: Academic Press; 1972;p. 243–314
  24. Kingery WD, Bowen HK, Uhlmann DR. Introduction to ceramics. New York: John Wiley and Sons; 1976;p. 768–815
  25. Della Bona A, van Noort R. Ceramic surface preparations for resin bonding. Am J Dent. 1998;11:276–280
  26. Jones DW. A brief overview of dental ceramics. J Can Dent Assoc. 1998;64:648–672
  27. Della Bona A, Anusavice KJ. Properties of dental ceramics. Int J Prosthodont. 2002;15:158–167

PII: S0109-5641(06)00078-9

doi: 10.1016/j.dental.2006.03.002

Dental Materials
Volume 23, Issue 4 , Pages 461-468 , April 2007