Dental Materials
Volume 23, Issue 4 , Pages 461-468 , April 2007

The impact of hydrofluoric acid surface treatments on the performance of a porcelain laminate restorative material

  • Owen Addison

      Affiliations

    • Biomaterials Unit, University of Birmingham, School of Dentistry, St. Chad's Queensway, Birmingham B4 6NN, UK
    • Corresponding Author InformationCorresponding author at: Biomaterials Unit, University of Birmingham School of Dentistry, St. Chad's Queensway, Birmingham, UK. Tel.: +44 237 2911; fax: +44 237 2932.
  • ,
  • Peter M. Marquis

      Affiliations

    • Biomaterials Unit, University of Birmingham, School of Dentistry, St. Chad's Queensway, Birmingham B4 6NN, UK
  • ,
  • Garry J.P. Fleming

      Affiliations

    • Materials Science Unit, Division of Oral Biosciences, Dublin Dental School and Hospital, Trinity College Dublin, Dublin 2, Republic of Ireland

Received 16 November 2005 ,Revised 23 February 2006 ,Accepted 9 March 2006.

To access this article, please choose from the options below

Login to an existing account or Register a new account.

  • Purchase this article for 31.50 USD (You must login/register to purchase this article)

    Online access for 24 hours. The PDF version can be downloaded as your permanent record.

  • Subscribe to this title

    Get unlimited online access to this article and all other articles in this title 24/7 for one year.

  • Claim access now

    For current subscribers with Society Membership or Account Number.

  • Visit SciVerse ScienceDirect to see if you have access via your institution.

PII: S0109-5641(06)00078-9

doi: 10.1016/j.dental.2006.03.002

Dental Materials
Volume 23, Issue 4 , Pages 461-468 , April 2007