Dental Materials
Volume 22, Issue 8 , Pages 771-777 , August 2006

The in vitro failure of all-ceramic crowns and the connector area of fixed partial dentures using bilayered ceramic specimens: The influence of core to dentin thickness ratio

  • Garry J.P. Fleming

      Affiliations

    • Materials Science Unit, Division of Oral Bioscience, Dublin Dental School & Hospital, University of Dublin, Trinity College, Lincoln Place, Dublin 2, Ireland
    • Corresponding Author InformationCorresponding author. Tel.: +353 1 612 7371; fax: +353 1 612 7371.
  • ,
  • Michelle Dickens

      Affiliations

    • Biomaterials Unit, School of Dentistry, University of Birmingham, St. Chad's Queensway, Birmingham B4 6NN, UK
  • ,
  • Laura J. Thomas

      Affiliations

    • Biomaterials Unit, School of Dentistry, University of Birmingham, St. Chad's Queensway, Birmingham B4 6NN, UK
  • ,
  • Jonathan J. Harris

      Affiliations

    • Biomaterials Unit, School of Dentistry, University of Birmingham, St. Chad's Queensway, Birmingham B4 6NN, UK

Received 8 April 2005 ,Revised 8 September 2005 ,Accepted 10 October 2005.

References 

  1. McLean JW, Hughes TH. The reinforcement of dental porcelain with ceramic oxides. Br Dent J. 1965;119:251–267
  2. Marquis PM. The Influence of Cements on the Mechanical Performance of Dental Ceramics. Proceedings of the fifth international symposium on ceramics in medicine. Bioceramics. 1992;5:317–324
  3. al-Shehri SA, Mohammed H, Wilson CA. Influence of lamination on the flexural strength of a dental castable glass ceramic. J Prosthet Dent. 1996;76:23–28
  4. Kappert HF, Knode H. In-Ceram: testing a new ceramic material. QDT. 1993;16:87–97
  5. Christiansen S, Albrecht M, Strunk HP, Hornberger H, Marquis PM, Franks J. Mechanical properties and microstructural analysis of a diamond-like carbon coating on an alumina/glass composite. J Mater Res. 1996;11:1934–1942
  6. White SN, Miklus VG, McLaren EA, Lang LA, Caputo AA. Flexural strength of a layered zirconia and porcelain dental all-ceramic system. J Prosthet Dent. 2005;94:125–131
  7. Hauptmann H, Reusch B. Investigation of connector cross-sections for 4-unit zirconia oxide bridges. J Dent Res. 2003;82;Abstr. No. 723
  8. White SN, Caputo AA, Vidjak FMA , Seghi RR. Moduli of rupture of layered dental ceramics. Dent Mater. 1994;10:52–58
  9. Lawn BR, Deng Y, Lloyd IK, Janal MN, Rekow ED, Thompson VP. Materials design of ceramic-based layer structures for crowns. J Dent Res. 2002;81:433–438
  10. Lawn BR, Deng Y, Miranda P, Pajares A, Chai H, Kim DK. Overview: damage in brittle layer structures from concentrated loads. J Mater Res. 2002;17:3019–3036
  11. Chai H, Lawn BR, Wuttiphan S. Fracture modes in brittle coatings with large interlayer modulus mismatch. J Mater Res. 1999;14:3805–3817
  12. Deng Y, Miranda P, Pajares A, Lawn BR. Fracture of ceramic/ceramic/polymer trilayers for biomechanical applications. J Biomed Mater Res. 2003;67A:828–833
  13. Lawn BR, Pajares A, Zhang Y, Deng Y, Polack MA, Lloyd IK, et al. Materials design in the performance of all-ceramic crowns. Biomaterials. 2004;25:2885–2992
  14. Lawn BR, Deng Y, Thompson VP. Use of contact testing in the characterization and design of all-ceramic crown-like layer structures: a review. J Prosthet Dent. 2001;86:495–510
  15. Fleming GJP, El-lakwah SFA, Harris JJ, Marquis PM. The effect of layer height variation on the bi-axial flexure strength and mode of failure of bilayered dental ceramics. Dent Mater. 2005;21:164–171
  16. Fleming GJP, El-lakwah SFA, Harris JJ, Marquis PM. The influence of interfacial surface roughness on bilayered ceramics performance. Dent Mater. 2004;20:142–149
  17. Fleming GJP, Nolan L, Harris JJ. In vitro clinical failure of an all-ceramic crown and connector area of a fixed partial denture using bilayered ceramic specimens: the influence of interfacial surface roughness. J Dent. 2005;33:405–412
  18. Fleming GJP, Shelton RM, Marquis PM. The influence of clinically induced variability on the bi-axial fracture strength of aluminous core porcelain discs. J Dent. 1999;27:587–594
  19. Fleming GJP, Addison O. The influence of cement lute, thermocycling and surface preparation on the strength of a porcelain laminate veneering material. Dent Mater. 2004;20:286–292
  20. Fleming GJP, Jandu HS, Nolan L, Shaini FJ. The influence of alumina abrasion and cement lute on the strength of a porcelain laminate veneering material. J Dent. 2004;32:67–74
  21. Anusavice KJ, Lee RB. Effect of firing temperature and water exposure on crack propagation in unglazed porcelain. J Dent Res. 1989;68:1075–1081
  22. Fleming GJP, Shaini FJ, Marquis PM. An assessment of the influence of mixing induced variability on the bi-axial flexure strength of dentine porcelain discs and the implications for laboratory testing of porcelain specimens. Dent Mater. 2000;16:114–119
  23. Thompson GA. Influence of relative layer height and testing method on the failure mode and origin in a bilayered dental ceramic composite. Dent Mater. 2000;16:235–243
  24. Zeng K, Odén A, Rowcliffe D. Evaluation of mechanical properties of dental ceramic materials in combination with porcelain. Int J Prosthodont. 1998;11:183–189
  25. Kelly JR, Tesk JA, Sorenson JA. Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modelling. J Dent Res. 1995;74:1253–1258
  26. Weibull W. A statistical distribution function of wide applicability. J Appl Mech. 1951;18:293–297
  27. Carrier DD, Kelly JR. In-Ceram failure behavior and core-veneer interface quality as influenced by residual infiltration glass. J Prosthodont. 1995;4:237–242
  28. Cazzato A, Faber KT. Fracture energy of glass-alumina interfaces via the bimaterial bend test. J Am Ceram Soc. 1997;80:181–188
  29. Evans AG, Hutchinson JW. Effects of nonplanarity on the mixed mode fracture resistance of bimaterial interfaces. Acta Metall Mater. 1989;37:909–916
  30. Wakabayashi N, Anusavice KJ. Crack initiation modes in bilayered alumina/porcelain disks as a function of core/veneer thickness ratio and supporting substrate stiffness. J Dent Res. 2000;79:1398–1404
  31. Wuttiphan S, Lawn BR, Padture NP. Crack suppression in strongly bonded homogeneous/heterogeneous laminates: a study on glass/glass-ceramic bilayers. J Am Ceram Soc. 1996;79:634–640
  32. Anusavice KJ, Hojjatie B. Tensile stress in glass-ceramic crowns: effect of flaws and cement voids. Int J Prosthodont. 1992;5:351–358
  33. Guazzato M, Proos K, Sara G, Swain MV. Strength, reliability and mode of fracture of bilayered porcelain/core ceramics. Int J Prosthodont. 2004;17:142–149
  34. Kelly JR, Campbell SD, Bowen HK. Fracture-surface analysis of dental ceramics. J Prosthet Dent. 1989;62:536–541
  35. Kelly JR, Giordano R, Pober R, Cima MJ. Fracture surface analysis of dental ceramics: clinically failed restorations. Int J Prosthodont. 1990;3:430–440

PII: S0109-5641(05)00288-5

doi: 10.1016/j.dental.2005.11.005

Dental Materials
Volume 22, Issue 8 , Pages 771-777 , August 2006