Dental Materials
Volume 22, Issue 4 , Pages 330-337 , April 2006

Surface analysis of porcelain fused to metal systems

Received 15 July 2004 ,Revised 13 April 2005 ,Accepted 12 May 2005.

References 

  1. O'Brien WJ, Ryge G. Relation between molecular force calculation and observed strengths of enamel-metal interfaces. J Am Ceram Soc. 1964;47:5–8
  2. Anusavice KJ, Horner JA, Fairhurst CW. Adherence controlling elements in ceramic-metal systems. I Precious alloys. J Dent Res. 1977;56:1045–1052
  3. Anusavice KJ, Ringle RD, Fairhurst CW. Adherence controlling elements in ceramic–metal systems, II nonprecious alloys. J Dent Res. 1977;56:1053–1061
  4. Cai Z, Watanabe I, Mitchell JC, Okabe T. X-ray diffraction investigation of metal–ceramic interfaces. J Dent Res. 1998;77:165
  5. Sarker NK, Verrett M, Eyer CS, Jeansonne EE. Role of gallium in alloy-porcelain bonding. J Prothet Dent. 1985;53:190–194
  6. Wagner WC, Asgar K, Bigelow WC, Flinn A. Effect of interfacial variables on metal–porcelain bonding. J Biomater Mater Res. 1993;27:531–537
  7. Pask JA, Tomsia AP. Oxidation and ceramic coatings on 80Ni20Cr alloys. J Dent Res. 1988;67:1164–1171
  8. Ringle RD, Fairhurst CW, Anusavice KJ. Microstructures in non-precious alloys near the porcelain–metal interaction zone. J Dent Res. 1979;58:1987–1993
  9. Wu Y, Moser JB, Jameson LM, Malone WFP. The effect of oxidation heat treatment on porcelain bond strength in selected base metal alloys. J Prosthet Dent. 1991;66:439–444
  10. Radnoth Von MS, Lautenschlager EP. Metal changes during porcelain firing. J Dent Res. 1969;48:321–324
  11. Brantley WA, Cai Z, Papazoglou E, Mitchell JC, Kerber SJ, Mann GP, et al. X-ray diffraction studies of oxidized high-palladium alloys. Dent Mater. 1996;12:333–341
  12. Diaz-Arnold AM, Keller JC, Wightman JP, Williams VD. Bond strength and surface characterization of a Ni–Cr–Be alloy. Dent Mater. 1996;12:58–63
  13. Kurisaki Y, Nagayama K. Influence of metal elements in Pd alloys on the bonding to porcelain. Shika Zairyo Kikai. 1990;9:11–29[English abstract]
  14. Hegedus C, Daroczi L, Kokenyesi V, Beke DL. Comparative microstructural study of the diffusion zone between NiCr alloy and different dental ceramics. J Dent Res. 2002;81:334–337
  15. Ohno H, Araki Y, Endo K. ESCA study on dental alloy surfaces modified by Ga–Sn alloy. J Dent Res. 1992;71:1332–1339
  16. Smith TB, Kelly JR, Tesk JA. In vitro fracture behaviour of ceramic and metal–ceramic restorations. J Prosthodont. 1994;3:138–144
  17. Carter JM, Mudafar-Al J, Sorensen SE. Adherence of a nickel–chromium alloy and porcelain. J Prosthet Dent. 1979;41:167–172
  18. Briggs D, Seah MP. Practical surface analysis. 2nd ed.. Auger and X-ray photoelectron spectroscopy. vol. 1. Chichester: Wiley; 1990;
  19. Askeland DR. The science of engineering materials. 3rd ed.. Cheltenham: Stanley Thornes Ltd; 1998;
  20. Papadopoulos T, Tsetsekou A, Eliades G. Effect of aluminium oxide sandblasting on cast commercially pure titanium surfaces. Eur J Prosthodont Restor Dent. 1999;7:15–21
  21. In:  Anusavice KJ editors. Science of dental materials. 10th ed.. Philadelphia: WB Saunders Co; 1996;
  22. Darvell BW, Samman N, Luk WK, Clark RK, Tideman H. Contamination of titanium castings by aluminium oxide blasting. J Dent. 1995;23:319–322

PII: S0109-5641(05)00180-6

doi: 10.1016/j.dental.2005.05.003

Dental Materials
Volume 22, Issue 4 , Pages 330-337 , April 2006