Dental Materials
Volume 22, Issue 3 , Pages 283-290 , March 2006

Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: The effect of surface conditioning

  • Regina Amaral

      Affiliations

    • São Paulo State University, Department of Dental Materials and Prosthodontics, São José dos Campos, Brazil
  • ,
  • Mutlu Özcan

      Affiliations

    • Faculty of Medical Sciences, Department of Dentistry and Dental Hygiene, Antonius Deusinglaan, University of Groningen, Groningen, The Netherlands
    • Corresponding Author InformationCorresponding author. Tel.:+31 50 363 8528; fax: +31 50 363 2696.
  • ,
  • Marco Antonio Bottino

      Affiliations

    • São Paulo State University, Department of Dental Materials and Prosthodontics, São José dos Campos, Brazil
  • ,
  • Luiz Felipe Valandro

      Affiliations

    • Federal University of Santa Maria, Department of Restorative Dentistry, Santa Maria, Brazil

Received 6 January 2005 ,Accepted 7 April 2005.

References 

  1. Calamia JR. Etched porcelain veneers: the current state of the art. Quintessence Int. 1985;1:5–12
  2. Stangel I, Nathanson D, Hsu CS. Shear strength of the composite bond to etched porcelain. J Dent Res. 1987;66:1460–1465
  3. Thurmond JW, Barkmeier W, Wilwerding TM. Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain. J Prosthet Dent. 1994;72:355–359
  4. Tylka DF, Stewart G. Comparison of acidulated phosphate fluoride gel and hydrofluoric acid etchants for porcelain-composite repair. J Prosthet Dent. 1994;72:121–127
  5. Aida M, Hayakawa T, Mizukawa K. Adhesion of composite to porcelain with various surface conditions. J Prosthet Dent. 1995;73:464–470
  6. Nicholls JI. Tensile bond to resin cements to porcelain veneers. J Prosthet Dent. 1998;60:443–447
  7. Rosenstiel SF, Gupta PK, Van der Sluys RA, Zimmermann MH. Strength of a dental glass-ceramic after surface coating. Dent Mater. 1993;9:274–279
  8. Wolf DM, Powers JM, O'Keefe KL. Bond strength of composite to etched and sandblasted porcelain. Am J Dent. 1993;6:155–158
  9. Kern M, Thompson VP. Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability. J Prosthet Dent. 1995;73:240–249
  10. Özcan M, Vallittu PK. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater. 2003;19:725–731
  11. Lu YC, Tseng H, Shih YH, Lee SY. Effects of surface treatments on bond strength of glass-infiltrated ceramic. J Oral Rehabil. 2001;28:805–813
  12. Özcan M, Alkumru HN, Gemalmaz D. The effect of surface treatment on the shear bond strength of luting cement to a glass-infiltrated alumina ceramic. Int J Prosthodont. 2001;14:335–339
  13. Kern M, Wegner SM. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater. 1998;14:64–71
  14. Derand P, Derand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont. 2000;13:131–135
  15. Sadoun M, Asmussen E. Bonding of resin cements to an aluminous ceramic: a new surface treatment. Dent Mater. 1994;10:185–189
  16. Özcan M, Pfeiffer P, Nergiz İ. A brief history and current status of metal/ceramic surface conditioning concepts for resin bonding in dentistry. Quintessence Int. 1998;29:713–724
  17. Strub JR, Stiffler S, Scharer P. Causes of failure following oral rehabilitation: biological versus technical factors. Quintessence Int. 1988;19:215–222
  18. Libby G, Arcuri MR, La Velle WE, Hel L. Longevity of fixed partial dentures. J Prosthet Dent. 1997;78:127–131
  19. Sorensen JA, Kang SK, Torres TJ, Knode H. In-ceram fixed partial dentures: three-year clinical trial results. J Californian Dent Assoc. 1998;26:207–214
  20. Peutzfeldt A, Asmussen E. Silicoating. Evaluation of a new method of bonding composite resin to metal. Scand J Dent Res. 1988;96:171–176
  21. Özcan M. The use of chairside silica coating for different dental applications. J Prosthet Dent. 2002;87:469–472
  22. Blatz MB, Sadan A, Kern M. Resin–ceramic bonding: a review of the literature. J Prosthet Dent. 2003;89:268–274
  23. Özcan M. Evaluation of alternative intraoral repair techniques for fractured ceramic-fused-to-metal restorations. J Oral Rehabil. 2003;30:194–203
  24. Andersson M, Oden A. A new all-ceramic crown-A dense-sintered, high purity alumina coping with porcelain. Acta Odontol Scand. 1993;51:59–64
  25. Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials. 1999;20:1–25
  26. Strub JR, Stiffler S, Scharer P. Causes of failure following oral rehabilitation: biological versus technical factors. Quintessence Int. 1988;19:215–222
  27. Shimada Y, Yamaguchi S, Tagami J. Micro-shear bond strength of dual-cured resin cement to glass ceramics. Dent Mater. 2002;18:380–388
  28. Della Bona A, van Noort R. Shear vs. tensile bond strength of resin composite bonded to ceramic. J Dent Res. 1995;74:1591–1596
  29. Cardoso PE, Sadek FT, Goracci C, Ferrari M. Adhesion testing with the microtensile method: effects of dental substrate and adhesive system on bond strength measurements. J Adhes Dent. 2002;4:291–297
  30. El Zohairy AA, De Gee AJ, Mohsen MM, Feilzer AJ. Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks.5. Dent Mater. 2003;19
  31. Özcan M. Adhesion of resin composites to biomaterials in dentistry: an evaluation of surface conditioning methods. 2003;Groningen, The Netherlands, p. 143–51
  32. Della Bona A, Anusavice KJ, Shen C. Microtensile strength of composite bonded to hot-pressed ceramics. J Adhesive Dent. 2000;2:305–313
  33. Denry IL, Mackert JR, Holloway JA, Rosenstiel SF. Effect of cubic leucite stabilization on the flexural strength of feldspathic dental porcelain. J Dent Res. 1996;75:1928–1935
  34. Mackert JR, Russell CM. Leucite crystallization during processing of a heat-pressed dental ceramic. Int J Prosthodont. 1996;9:261–265
  35. Mackert JR, Williams AL, Ergle JW, Russell CM. Water-enhanced crystallization of leucite in dental porcelain. Dent Mater. 2000;16:426–431
  36. Probster L, Diehl J. Slip-casting alumina ceramics for crown and bridge restorations. Quintessence Int. 1992;23:25–31
  37. Özcan M, Lassila L, Raadschelders J, Matinlinna JP, Vallittu PK. Effect of some parameters on silica-deposition on a zirconia ceramic. J Dent Res. 2005;84:(Abstract# 545)

PII: S0109-5641(05)00173-9

doi: 10.1016/j.dental.2005.04.021

Dental Materials
Volume 22, Issue 3 , Pages 283-290 , March 2006